Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.8 min @Temperature 155 °C |
0.180 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 10.8 min @Temperature 155 °C |
0.180 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 6.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |