Polymer Property : Hold Pressure = 700 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 4.83 MPa

@Time 15.0 sec
700 psi

@Time 0.00417 hour
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e..
Hold Pressure 4.83 MPa

@Time 15.0 sec
700 psi

@Time 0.00417 hour
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b..
Hold Pressure 4.83 MPa

@Time 10.0 sec
700 psi

@Time 0.00278 hour
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer
PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist..