Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 4.83 MPa @Time 15.0 sec |
700 psi @Time 0.00417 hour |
|
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Hold Pressure | 4.83 MPa @Time 15.0 sec |
700 psi @Time 0.00417 hour |
|
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
Hold Pressure | 4.83 MPa @Time 10.0 sec |
700 psi @Time 0.00278 hour |
|
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |