Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 34.5 - 68.9 MPa | 5000 - 10000 psi | Injection |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Hold Pressure | 34.5 - 68.9 MPa | 5000 - 10000 psi | Injection |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Hold Pressure | 34.5 - 68.9 MPa | 5000 - 10000 psi | Injection |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Hold Pressure | 34.5 - 68.9 MPa | 5000 - 10000 psi | Injection |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Hold Pressure | 34.5 - 68.9 MPa | 5000 - 10000 psi | Injection |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |