Polymer Property : Extrusion Rate = 78.0 g/min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Extrusion Rate 78.0 g/min
78.0 g/min
3 bar, 3mm aperture
Dow BETAMATE™ 5103-2 Epoxy
BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste..