Polymer Property : Gel Time = 3.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 3.00 min

@Temperature 135 °C
3.00 min

@Temperature 275 °F
0% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 138 °C
3.00 min

@Temperature 280 °F
23.17% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 140 °C
3.00 min

@Temperature 284 °F
25.7% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 143 °C
3.00 min

@Temperature 289 °F
53.3% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 145 °C
3.00 min

@Temperature 293 °F
43.5% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 148 °C
3.00 min

@Temperature 298 °F
71.81% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 150 °C
3.00 min

@Temperature 302 °F
79.16% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 153 °C
3.00 min

@Temperature 307 °F
80.27% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 min

@Temperature 155 °C
3.00 min

@Temperature 311 °F
83.62% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 3.00 - 4.00 min

@Temperature 140 °C
3.00 - 4.00 min

@Temperature 284 °F
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.
Gel Time 3.00 min

@Temperature 135 °C
3.00 min

@Temperature 275 °F
Hexcel® HexPly® EH04 Epoxy Resin System
HexPly® EH04 is a modified epoxy resin system specifically designed for bladder molding or sheet wrap tube applications. Unique chemistry provides full cured parts in only 3 minutes at 138°C.Appli..