Gel Time 15.0 min

@Temperature 135 °C
15.0 min

@Temperature 275 °F
79.98% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 138 °C
15.0 min

@Temperature 280 °F
83.72% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 140 °C
15.0 min

@Temperature 284 °F
86.78% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 143 °C
15.0 min

@Temperature 289 °F
87.12% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 145 °C
15.0 min

@Temperature 293 °F
89.11% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 148 °C
15.0 min

@Temperature 298 °F
89.94% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 150 °C
15.0 min

@Temperature 302 °F
89.6% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 153 °C
15.0 min

@Temperature 307 °F
89.41% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 min

@Temperature 155 °C
15.0 min

@Temperature 311 °F
90.16% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 15.0 - 20.0 min

@Temperature 50.0 °C
15.0 - 20.0 min

@Temperature 122 °F
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive
Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu..