Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.666666 - 1.00 min @Temperature 232 °C |
0.666666 - 1.00 min @Temperature 450 °F |
|
3M Scotchkote™ 206N XTRA LG Fusion Bonded Epoxy Coating Scotchkote Fusion Bonded Epoxy coating 206N XTRA LG is one-part, heat curable, thermosetting, powdered epoxy coating with extended gel for coating the interior of line pipe and fittings, valves, and.. |