Processing Properties | Metric | English | Comments |
---|---|---|---|
Solution Temperature | 128 °C | 262 °F | DIN 54 408, modified |
The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined wi.. |