Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1350 °C | 2460 °F | |
Wieland Porta P6 PFM Alloy Gold-platinum-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental |
|||
Casting Temperature | 1350 °C | 2460 °F | |
Wieland Simidur S 1S PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |