Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1080 - 1130 °C | 1980 - 2070 °F | |
Wieland 1914 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Casting Temperature | 1080 °C | 1980 °F | |
Wieland Portadur P2 Casting Alloy Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |