Polymer Property : Casting Temperature = 1080 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 1080 - 1130 °C
1980 - 2070 °F
Wieland 1914 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental
Casting Temperature 1080 °C
1980 °F
Wieland Portadur P2 Casting Alloy
Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental