Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1010 - 1110 °C | 1850 - 2030 °F | |
Wieland 1007 Wilaform Gold Silver white gold alloy for all kinds of decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, tubingDental |
|||
Casting Temperature | 1010 - 1110 °C | 1850 - 2030 °F | |
Wieland 1023 Wilaform Gold Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental |
|||
Casting Temperature | 1010 - 1110 °C | 1850 - 2030 °F | |
Wieland 1602 Wilaform Gold Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu.. |
|||
Casting Temperature | 1010 - 1100 °C | 1850 - 2010 °F | |
Wieland 3013 Wilaform Silver Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental |