Processing Properties Metric English Comments
Casting Temperature 960 - 1060 °C
1760 - 1940 °F
Wieland 1910 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental