Processing Properties Metric English Comments
Casting Temperature 1050 - 1150 °C
1920 - 2100 °F
Wieland 1601 Wilaform Gold
Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, ..
Casting Temperature 1050 °C
1920 °F
Wieland Portadur T Casting Alloy
Gold casting alloyApplications: inlays/onlays, crowns, acrylic veneeringDental