Polymer Property : Zone 5 = 509 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 5 265 °C
509 °F
Honeywell Aegis™ HFX High Barrier Nylon  (discontinued **)
Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is ..