Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 260 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4300 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4612R PBT, 7% Glass Reinforced  (Unverified Data**)
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Vandar 4632Z is a high impact, 15% glass reinforced polyester alloy. It combines high strength and toughness with a moderate degree of rigidity. It is characterized by excellent solvent resistance, ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1400A PBT, Unfilled
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2000-3 PBT, Unfilled
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2004-2 PBT, Unfilled
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2401 MT PBT, Medical Technology
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3200-2 PBT, 15% Glass Reinforced
Celanex 3200-2 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3200-2 contains an internal lubricant.In..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese CELANEX 3309HRT PBT, 30% Glass Reinforced
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003-2 PBT, Unfilled
Celanex 2003-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-2 is a medium h..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less tha..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty
40% long carbon fiber reinforced Thermoplastic PolyurethaneInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese VANDAR 4602Z PBT, Unfilled
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 531HS PBT, Glass Reinforced
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3209HRT PBT, 15% Specialty
Celanex 3209HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate material that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celane..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese Celanex® 3325HRT PBT, 30% Glass Reinforced
Celanex 3325HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at bre..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced  (Unverified Data**)
40% long strand glass fiber reinforced thermoplastic polyurethane40% long strand glass fiber reinforced thermoplastic polyurethaneCelstran can be processed on a standard injection molding unit.Infor..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 4302LM PBT, 30% Glass Reinforced
Celanex 4302LM is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.Information provided b..
Copyright © lookpolymers.com All Rights Reserved