Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 500 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1400A PBT  (Unverified Data**)
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1600A PBT  (Unverified Data**)
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Extrusion gradeInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2002-3 PBT  (Unverified Data**)
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced  (Unverified Data**)
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.7.5% glass-f..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3200-2FC PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.30% glass fiber, good impact strength, laser markableInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1400A PBT, Unfilled
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1600FC PBT, Unfilled
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1632Z PBT, 15% Glass Reinforced
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2000-3 PBT, Unfilled
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2002-3 PBT, Unfilled
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2004-2 PBT, Unfilled
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3400-2 PBT, 40% Glass Reinforced
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 4300 PBT, 30% Glass Reinforced
Celanex 4300 is a toughened, 30% glass reinforced PBT.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003-2 PBT, Unfilled
Celanex 2003-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-2 is a medium h..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3300-2LM PBT, Glass Reinforced
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available i..
Zone 4 245 - 260 °C
473 - 500 °F
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Vandar® 2100UV PBT, Impact Modified  (Unverified Data**)
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese VANDAR 2122 PBT, 10% Mineral Reinforced
Vandar 2122 is a polyester alloy which contains 10% mineral filler. It offers exceptional toughness and practical impact strength. This resin offers Class A paintable finish with excellent dimension..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese VANDAR 4662Z PBT, 30% Glass Reinforced
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Copyright © lookpolymers.com All Rights Reserved