Polymer Property : Zone 2 = 680 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 - 380 °C
680 - 716 °F
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 2 360 °C
680 °F
Compression
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Zone 2 360 °C
680 °F
Compression
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
Zone 2 360 °C
680 °F
Compression
BASF Ultrason® P 3010 MR SW 10101 PPSU
Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati..
Zone 2 360 °C
680 °F
Compression
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..