Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 300 °C | 572 °F | Compression |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Zone 2 | 300 °C | 572 °F | Compression |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |