Polymer Property : Zone 2 = 230 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 110 - 130 °C
230 - 266 °F
Solvay Specialty Polymers Cogegum® GFR/380 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..