Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 110 - 130 °C | 230 - 266 °F | |
Solvay Specialty Polymers Cogegum® GFR/380 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |