Processing Properties Metric English Comments
Die Temperature 185 - 193 °C
365 - 379 °F
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..
Die Temperature 182 - 193 °C
360 - 379 °F
Zone 1, Extrusion
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..