Processing Properties Metric English Comments
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 2016 PBT  (Unverified Data**)
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3216 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 4016 PBT  (Unverified Data**)
Non-exuding, unfilled, flame retardant polybutylene terephthalate which has an excellent balance of mechanical properties and processability. Celanex 4016 is well suited for applications requiring i..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese Celanex® 7716 PBT, 35% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese Vandar® 8000 PBT  (Unverified Data**)
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 215 - 255 °C
419 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 255 °C
428 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 250 - 255 °C
482 - 491 °F
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 2016 PBT, Unfilled
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese CELANEX 3216HR PBT, 15% Glass Reinforced
Celanex 3216HR is a flame retarded, hydrolysis resistant, 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information ..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese CELANEX 3316HR PBT, 30% Glass Reinforced
Celanex 3316HR is a flame retarded, hydrolysis resistant, 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3314 PBT, 30% Glass Reinforced
Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced
Celanex 7316 is a non-exuding (UL and CSA approved V-0 at 1/32 inch), 35% glass/mineral reinforced PBT, which has an excellent balance of mechanical properties and processability. It is well suited..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 4016 PBT, Unfilled
Non-exuding, unfilled, flame retardant polybutylene terephthalate which has an excellent balance of mechanical properties and processability. Celanex 4016 is well suited for applications requiring i..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese VANDAR 8000 PBT, Unfilled
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Die Temperature 240 - 255 °C
464 - 491 °F
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced