Processing Properties Metric English Comments
Adapter Temperature 325 - 370 °C
617 - 698 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st..
Adapter Temperature 325 - 370 °C
617 - 698 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..