Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 325 - 370 °C | 617 - 698 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Adapter Temperature | 325 - 370 °C | 617 - 698 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |