Polymer Property : Adapter Temperature = 338 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 170 - 180 °C
338 - 356 °F
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film
The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar..
Adapter Temperature 170 - 190 °C
338 - 374 °F
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer
The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica..
Adapter Temperature 170 - 190 °C
338 - 374 °F
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer
The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high ..
Adapter Temperature 170 °C
338 °F
Extrusion
Huntsman IROGRAN® CA116-201 TPU-Polyester
Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee..
Adapter Temperature 170 °C
338 °F
5, Extrusion
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane
Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, ..
Adapter Temperature 170 °C
338 °F
5
Lubrizol Estane® 54601 Thermoplastic Polyurethane
Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A..