Polymer Property : Adapter Temperature = 191 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 191 °C
376 °F
Extrusion
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane
Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Adapter Temperature 191 °C
376 °F
5, Extrusion
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am..