Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 35.0 °C | 95.0 °F | |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |