Processing Properties Metric English Comments
Feed Temperature 154 - 163 °C
310 - 325 °F
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene  (Unverified Data**)
ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Alathon® M5370WC High Density Polyethylene
ApplicationsALATHON M 5370WC is a natural, high density, polyethylene copolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cab..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..
Feed Temperature 154 - 163 °C
310 - 325 °F
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to..
Feed Temperature 154 - 163 °C
310 - 325 °F
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm..
Feed Temperature 154 - 163 °C
310 - 325 °F
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene
ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® KR92717 High Density Polyethylene
ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® KR92828 High Density Polyethylene
ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont..
Feed Temperature 154 - 163 °C
310 - 325 °F
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene
ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant ..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR590001 High Density Polyethylene
ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR590005 High Density Polyethylene
ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains ..
Feed Temperature 149 - 163 °C
300 - 325 °F
LyondellBasell Petrothene® LR686001 High Density Polyethylene
ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen..
Feed Temperature 154 - 163 °C
309 - 325 °F
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled
Data provided by Clariant Masterbatches