Feed Temperature 245 - 260 °C
473 - 500 °F
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di..
Feed Temperature 245 - 255 °C
473 - 491 °F
Lavergne VYPET VNT 1020 Polyester-PC Alloy
The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
Feed Temperature 245 - 255 °C
473 - 491 °F
Lavergne VYPET VNT 1021 Polyester-PC Alloy
The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..