Processing Properties Metric English Comments
Feed Temperature 210 °C
410 °F
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer
PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mech..
Feed Temperature 210 - 230 °C
410 - 446 °F
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5..
Feed Temperature 210 - 225 °C
410 - 437 °F
Lubrizol Estane® S375D Thermoplastic Polyurethane
Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..