Processing Properties Metric English Comments
Zone 4-x 177 °C
350 °F
LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer
ApplicationsAQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after..
Zone 4-x 177 °C
350 °F
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
ApplicationsAQUATHENE FR 4098-00 is a colorable flame retardant masterbatch designed specifically for moisture cure applications. When FR 4098-00 is combined with AQ 120-000 and CM 04482 in the cor..