Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Crosslinkable
Manufacturer LyondellBasell (former Equistar)
Trade Name Aquathene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAQUATHENE FR 4098-00 is a colorable flame retardant masterbatch designed specifically for moisture cure applications. When FR 4098-00 is combined with AQ 120-000 and CM 04482 in the correct ratio this formulation is suitable for use in 600-V power cable and control cable applications where UL44 horizontal flame rating and 90°C service in wet locations are required. When melt blended using 30 wt.% FR 4098-00, 5 wt.% CM 04482 and 65 wt.% AQ 120-000, this formulation is designed to meet the following UL requirements: SIS, XHHW, XHHW-2, RHH, RHW, and RHW-2. ProcessingThe moisture curable system of FR 4098-00, CM 04882 and AQ 120-000 can be extruded as wires and cable insulation using a conventional extruder. The total system, FR 4098-00, CM 04482 and AQ 120-000, crosslinks after the materials are mixed during extrusion and subsequently exposed to moisture. Crosslinking can be achieved by exposure to steam, immersion in water or storage at ambient conditions. Since cure time varies considerable with environmental conditions and cable constructions, contact your Equistar sales representative for detailed cure conditions. This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D1505
Melt Flow 0.70 g/10 min
0.70 g/10 min
ASTM D1238
Processing Properties Metric English Comments
Feed Temperature 146 °C
295 °F
Zone 2 154 °C
310 °F
Zone 3 163 °C
325 °F
Zone 4-x 177 °C
350 °F
Adapter Temperature 182 °C
360 °F
Die Temperature 182 °C
360 °F
Wire Preheat Temperature 104 °C
220 °F