Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 4.00 min @Temperature 23.9 °C |
4.00 min @Temperature 75.0 °F |
|
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges
(discontinued **) Features include fast cure adhesive, semi-rigid urethane, 15-20 minutes handling strength, and excellent gap filler and non sag product for wood and plastic. Mix ratio by volume 1:1. Average T-Peel.. |
|||
Pot Life | 4.00 - 10100 min | 4.00 - 10100 min | Average value: 428 min Grade Count:33 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Pot Life | 4.00 min @Temperature 25.0 °C |
4.00 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Pot Life | 4.00 - 7.00 min @Temperature 25.0 °C |
4.00 - 7.00 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2551 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 4.00 min @Temperature 23.9 °C |
4.00 min @Temperature 75.0 °F |
|
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |