Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 4.00 - 10100 min | 4.00 - 10100 min | Average value: 428 min Grade Count:33 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |