Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 3600 - 6000 min | 3600 - 6000 min | 100 gram mass |
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Pot Life | 3600 min | 3600 min | |
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al.. |
|||
Pot Life | 3600 min | 3600 min | |
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also .. |