Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 180 - 300 min | 180 - 300 min | |
Abatron AboThane 8901-4 Polyurethane Enamel Clear, glossy polyurethane enamel with good chemical, weather and abrasion resistance as a clear anti-graffiti coating. High-grade, high-build, 2-component system for good performance on metal, woo.. |