Processing Properties Metric English Comments
Pot Life 200 min
200 min
Abatron AboWeld 8201-14/AboCure 8201-14 Carbon-Filled Electrically Conductive Epoxy Compound
AboWeld 8201-14/AboCure 8201-14 is an easy-to-use and very conductive carbon-epoxy paste. As the size of the conductive particles is relatively coarse, this product is used primarily as a thick adhe..
Pot Life 200 min

@Temperature 100 °C
200 min

@Temperature 212 °F
Abatron AboCast 8504-1 One-Component Epoxy
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.