Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 2.0 - 2.5 min @Temperature 24.0 °C |
2.0 - 2.5 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products Proto-Kast BC 8163 Urethane Casting BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and.. |