Processing Properties Metric English Comments
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Time before parts must be mated
Lord Adhesives 360 Sag-Resistant, High-Performance, 5 min Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 2.0 - 3.0 min
2.0 - 3.0 min
Time before parts must be mated
Lord Adhesives 363 Two-Component, Fast Set, Modified Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Time before parts must be mated
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Time before parts must be mated
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
100 gram batch
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound
Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Work Life
Loctite® 3035™ Polyolefin Bonder
Loctite® 3035™ Polyolefin Bonder is an easy-to-use, 1:1 mix product that can be stored at room temperature and works where traditional low surface energy bonders often fail. Loctite® 3035™ Polyo..
Pot Life 2.0 - 2.5 min

@Temperature 24.0 °C
2.0 - 2.5 min

@Temperature 75.2 °F
1 lb. mass
BCC Products Proto-Kast BC 8163 Urethane Casting
BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Mass: 50g; TM R050-19
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Mass: 50g; TM R050-19
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..