Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 129600 min | 129600 min | |
Epoxy Technology EPO-TEK® ED1021 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil.. |
|||
Pot Life | 129600 min | 129600 min | |
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d.. |