Processing Properties Metric English Comments
Pot Life 0.50 - 0.75 min
0.50 - 0.75 min
Open Time
Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue Stick
Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue StickLow viscosity. Easy to gun. Long open time. Flexible, no cracking. Excellent bonding range.
Pot Life 0.50 - 0.75 min
0.50 - 0.75 min
Open Time
Bostik 6344 Low Temperature EVA Glue Stick
Bostik 6344 Low Temperature EVA Glue StickLong open time. Low temperature glue is safer to use. Bonds heat sensitive foams. Excellent bonds at lower temperatures.