Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 6328 Low Viscosity, Long Open Time, Flexible EVA Glue StickLow viscosity. Easy to gun. Long open time. Flexible, no cracking. Excellent bonding range.
Physical Properties Metric English Comments
Viscosity 10000 cP

@Temperature 177 °C
10000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.1 °C
151 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Processing Properties Metric English Comments
Pot Life 0.50 - 0.75 min
0.50 - 0.75 min
Open Time
Descriptive Properties Value Comments
Color Straw