Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 195 - 210 °C | 383 - 410 °F | Extrusion Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |