Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Kolon
Trade Name ELLAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Tensile Strength 49.0 MPa
7110 psi
ASTM D412
Tensile Stress 14.7 MPa

@Strain 100 %
2130 psi

@Strain 100 %
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
Tear Strength 167 kN/m
952 pli
ASTM D624
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Nozzle Temperature 195 - 205 °C
383 - 401 °F
Injection Molding
Zone 1 160 - 175 °C
320 - 347 °F
Injection Molding
160 - 175 °C
320 - 347 °F
Extrusion Molding
Zone 2 180 - 190 °C
356 - 374 °F
Injection Molding
185 - 195 °C
365 - 383 °F
Extrusion Molding
Zone 3 180 - 195 °C
356 - 383 °F
Extrusion Molding
185 - 195 °C
365 - 383 °F
Injection Molding
Zone 4 190 - 205 °C
374 - 401 °F
Extrusion Molding
Die Temperature 190 - 205 °C
374 - 401 °F
Extrusion Molding
Head Temperature 195 - 210 °C
383 - 410 °F
Extrusion Molding
Users viewing this material also viewed the following: