Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 113 - 118 °C | 235 - 245 °F | |
LyondellBasell Petrothene® XL07425 Copolymer ApplicationsPETROTHENE XL07425 is especially formulated for use in flame retardant primary insulation for low voltage automotive wire and cable applications (SAE J1128). Non-discoloring antioxidant .. |