Polymer Property : Head Temperature = 115 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 115 - 125 °C
239 - 257 °F
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen
E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond..