Processing Properties Metric English Comments
Hot-Working Temperature 899 - 1200 °C
1650 - 2200 °F
Uniformly heating
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..
Hot-Working Temperature >= 899 °C
>= 1650 °F
Forge
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..