Processing Properties | Metric | English | Comments |
---|---|---|---|
Hot-Working Temperature | 899 - 1200 °C | 1650 - 2200 °F | Uniformly heating |
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |
|||
Hot-Working Temperature | >= 899 °C | >= 1650 °F | Forge |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |